Mitsubishi · chipbreaker for negative inserts
MK chipbreaker
First recommendation for medium cutting of cast iron; balances sharpness and edge strength.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Negative
- Made for
- ISO K (cast iron)
- Cutting area
- medium
- Feed
- 0.2–0.56 mm/rev (.0079–.022 in/rev)
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
Mitsubishi’s first choice
- For gray cast iron, up to 350 MPa (e.g. Class 45 B), a medium cut: MK, with MC5105 (stable), MC5105 (general), MC5115 (unstable).
One source: Mitsubishi Materials, its own catalog
Open the insert pickerMK equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Seco | M5 | ISO K; medium | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
Why MK for gray cast iron
MK for gray cast iron: Mitsubishi’s medium geometry for ISO K.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi makes MK (negative) for K in medium at 0.2–0.56 mm/rev (.0079–.022 in/rev). First recommendation for medium cutting of cast iron; balances sharpness and edge strength.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [3]
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists MK for ISO K, medium. Mitsubishi Materials’ own catalog is the authority for its geometry.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)