Mitsubishi · chipbreaker for positive inserts
MM chipbreaker
First recommendation for medium cutting of stainless.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Positive
- Made for
- ISO M (stainless steel)
- Cutting area
- medium
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
MM equivalents
Other makers’ chipbreakers for positive inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | MP | ISO M; medium | 0.1–0.41 mm/rev | Medium machining of steel, stainless, cast iron and high-temperature alloys. | One source: Kennametal, its own catalog |
| Sandvik | MM | ISO M; medium | not printed | First choice for medium machining of stainless (CoroTurn 107). | One source: Sandvik Coromant, its own catalog |
Why MM for austenitic stainless (304, 316)
MM for austenitic stainless (304, 316): Mitsubishi’s medium geometry for ISO M.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi makes MM (positive) for M in medium. First recommendation for medium cutting of stainless.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists MM for ISO M, medium. Mitsubishi Materials’ own catalog is the authority for its geometry.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)