Kennametal · chipbreaker for positive inserts
MP chipbreaker
Medium machining of steel, stainless, cast iron and high-temperature alloys.
One source: Kennametal, its own catalog
What Kennametal prints
- Insert
- Positive
- Made for
- ISO P (steel), M (stainless steel), K (cast iron), S (superalloys and titanium)
- Cutting area
- medium
- Feed
- 0.1–0.41 mm/rev (.0039–.0161 in/rev)
- Depth of cut
- 0.41–3.3 mm (.016–.13 in)
Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)
MP equivalents
Other makers’ chipbreakers for positive inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Mitsubishi | MM | ISO M; medium | not printed | First recommendation for medium cutting of stainless. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MS | ISO S; medium | not printed | First recommendation for medium cutting of difficult-to-cut materials. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MV | ISO P, M; medium | not printed | Alternative for medium cutting of steel and stainless; large rake. | One source: Mitsubishi Materials, its own catalog |
| Sandvik | MM | ISO M; medium | not printed | First choice for medium machining of stainless (CoroTurn 107). | One source: Sandvik Coromant, its own catalog |
Why MP for steel
MP for steel: Kennametal’s medium geometry for ISO P.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal makes MP (positive) for P, M, K, S in medium at 0.1–0.41 mm/rev (.0039–.0161 in/rev). Medium machining of steel, stainless, cast iron and high-temperature alloys.
One source: Kennametal, the maker of the chipbreaker , sources [3]
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists MP for ISO P, M, medium. Kennametal’s own catalog is the authority for its geometry.
It agrees with Kennametal’s catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)