Mitsubishi · chipbreaker for positive inserts

MV chipbreaker

Alternative for medium cutting of steel and stainless; large rake.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a positive insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 7° clearance; made for ISO P and M.chipcutting edgebreaker grooveclearance 7°ISO groupPM
The edge in section; its ISO groups. Not to scale.

What Mitsubishi prints

Insert
Positive
Made for
ISO P (steel), M (stainless steel)
Cutting area
medium

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

MV equivalents

Other makers’ chipbreakers for positive inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalMPISO P, M; medium0.1–0.41 mm/revMedium machining of steel, stainless, cast iron and high-temperature alloys.

One source: Kennametal, its own catalog

SandvikMMISO M; mediumnot printedFirst choice for medium machining of stainless (CoroTurn 107).

One source: Sandvik Coromant, its own catalog

Why MV for steel

MV for steel: Mitsubishi’s medium geometry for ISO P.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Mitsubishi makes MV (positive) for P, M in medium. Alternative for medium cutting of steel and stainless; large rake.

    One source: Mitsubishi Materials, the maker of the chipbreaker , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists MV for ISO P, M, medium. Mitsubishi Materials’ own catalog is the authority for its geometry.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)