Mitsubishi · chipbreaker for negative inserts

RK chipbreaker

First recommendation for rough cutting of cast iron; stable in interrupted cuts and scale removal.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO K.chipcutting edgebreaker grooveclearance 0°ISO groupK
The edge in section; its ISO groups. Not to scale.

What Mitsubishi prints

Insert
Negative
Made for
ISO K (cast iron)
Cutting area
roughing
Edge
Wide land

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

Mitsubishi’s first choice

  • For gray cast iron, up to 350 MPa (e.g. Class 45 B), roughing: RK, with MC5105 (stable), MC5105 (general), MC5115 (unstable).

One source: Mitsubishi Materials, its own catalog

Open the insert picker

RK equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalRPISO K; roughingnot printedRoughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided).

One source: Kennametal, its own catalog

SecoM5ISO K; roughing0.3–0.7 mm/revRoughing with double-sided inserts at high feed in steel, stainless and cast iron.

One source: Seco Tools, its own catalog

Why RK for gray cast iron

RK for gray cast iron: Mitsubishi’s roughing geometry for ISO K.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Mitsubishi makes RK (negative) for K in roughing; edge: Wide land. First recommendation for rough cutting of cast iron; stable in interrupted cuts and scale removal.

    One source: Mitsubishi Materials, the maker of the chipbreaker , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists RK for ISO K, roughing. Mitsubishi Materials’ own catalog is the authority for its geometry.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)