Mitsubishi · chipbreaker for negative inserts
RP chipbreaker
First recommendation for rough cutting of carbon and alloy steel; interrupted cuts and removing scale.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Negative
- Made for
- ISO P (steel)
- Cutting area
- roughing
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
Mitsubishi’s first choice
- For carbon and alloy steel, 180–280 HB (e.g. 1045, 4140), roughing: RP, with MC6115 (stable), MC6125 (general), MC6025 (unstable).
One source: Mitsubishi Materials, its own catalog
Open the insert pickerRP equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | RP | ISO P; roughing | not printed | Roughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided). | One source: Kennametal, its own catalog |
| Seco | M5 | ISO P; roughing | 0.3–0.7 mm/rev | Roughing with double-sided inserts at high feed in steel, stainless and cast iron. | One source: Seco Tools, its own catalog |
| Seco | RR6 | ISO P; roughing | 0.3–1 mm/rev | Very easy-cutting single-sided roughing of stainless and steel. | One source: Seco Tools, its own catalog |
Why RP for steel
RP for steel: Mitsubishi’s roughing geometry for ISO P.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi makes RP (negative) for P in roughing. First recommendation for rough cutting of carbon and alloy steel; interrupted cuts and removing scale.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [3]
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists RP for ISO P, roughing. Mitsubishi Materials’ own catalog is the authority for its geometry.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)