ASME B16.5 · Class 300 (300#)

18" Class 300 flange: bolts and torque

An 18" Class 300 flange takes 24 studs, 1-1/4-8 UN, on a 24-3/4" bolt circle, 7-3/4" long for a raised face and 8-1/4" for a ring joint. With a spiral wound gasket and B7 studs the gasket makers' tables give 918 ft·lb per stud.

A Class 300 NPS 18 flange face on, to scale: 28" OD, 24 holes of 1-3/8" on a 24-3/4" bolt circle, each with a 1-1/4" stud.OD 28"bolt circle 24-3/4"hole 24 × 1-3/8"bolt 24 × 1-1/4"
The NPS 18 Class 300 flange, face on. To scale.

A starting point from published gasket-maker tables. Your site’s bolting procedure, or a PCC-1 qualified joint procedure, governs pressure piping.

Studs and flange

Studs
24 × 1-1/4-8 UN
Stud length, raised face
7-3/4" (1/16" raised face)
Stud length, ring joint
8-1/4"
Nut wrench
2" (heavy hex)
Bolt circle
24-3/4"
Flange OD
28"
Bolt holes
1-3/8"

Checked against 3 published copies

Stud lengths are measured first thread to first thread, as B16.5 lists them.

Torque by gasket

Per stud, ASTM A193 B7 studs with 2H nuts, lubricated as each maker's table assumes.

  • Spiral wound918 ft·lb · 1,244 N·m

    Garlock 1,000 · Flexitallic 750 · Teadit 835 · FNW 1,012 ft·lb (span 478–1,012)

    Median of 4 makers

  • Sheet (PTFE, graphite, fibre)686 ft·lb · 929 N·m

    Garlock 686 · Gore 750 · Thomson 615 ft·lb (span 371–1,000)

    Median of 3 makers

  • Ring joint (RTJ)915 ft·lb · 1,240 N·m

    Computed, no maker table: no gasket maker prints ring joint torque per flange size.

    How it's computed

    T = K × D × F at 60% of B7 yield (63 ksi) on the .929 in² root area, K 0.15.

Median of 3 makers

Work it in the calculator: other stud materials (B7M, L7, B8M), your lubricant's K, or your own bolt stress.

Passes (spiral wound, 918 ft·lb)

Passes for the spiral wound gasket, to 918 ft·lb
  1. Snug by hand, then a short wrench, in the star
  2. 30% in the star275 ft·lb
  3. 60–70% in the star551–642 ft·lb
  4. 100% in the star918 ft·lb
  5. Check bolt to bolt round the flange until no nut turns918 ft·lb

The passes as the gasket makers print them.

Tightening order for 24 bolts →

Gaskets for this flange

Spiral wound, sheet and ring joint sizes

Dimensions from ASME B16.20 (spiral wound, ring joint) and B16.21 (sheet), checked against published copies.

Units
Spiral wound
Inner ring ID17.69449.3
Winding ID × OD18.69474.7 × 20.75527.1
Centering ring OD23.50596.9
Inner ringNot required
Sheet ring
ID × OD18.00457.2 × 23.50596.9
Ring joint
Ring numberR-69

Sources