Class 300 spiral wound gasket dimensions

A Class 300 NPS 2 spiral wound gasket winds from 2.75" to 3.38" on a 4.38" centering ring. The four diameters of a spiral wound gasket with inner and centering rings, NPS 1/2 to 24. Each is checked against three published copies of the standard (two for the inner ring); a tag marks any size where they differ.

The Class 300 NPS 2 spiral wound gasket, face on, to scale: centering ring Ø4.38", winding Ø2.75"–3.38".centering ring Ø4.38"winding Ø2.75"–3.38"
The Class 300 NPS 2 spiral wound gasket, face on. To scale.
Units

Class 300 spiral wound gasket chart

Class 300 spiral wound gaskets: inner ring ID, winding ID and OD, centering ring OD by pipe size
NPSInner ring ID (inmm)Winding ID (inmm)Winding OD (inmm)Centering ring OD (inmm)Inner ring
1/20.5614.20.7519.11.2531.82.1354.0Not required
3/40.8120.61.0025.41.5639.72.6366.7Not required
11.0626.91.2531.81.8847.62.8873.0Not required
1-1/41.5038.11.8847.62.3860.33.2582.6Not required
1-1/21.7544.52.1354.02.7569.93.7595.3Not required
22.1955.62.7569.93.3885.74.38111.1Not required
2-1/22.6266.53.2582.63.8898.45.13130.2Not required
33.1981.04.00101.64.75120.75.88149.2Not required
44.19106.45.00127.05.88149.27.13181.0Not required
55.19131.86.13155.67.00177.88.50215.9Not required
66.19157.27.19182.68.25209.69.88250.8Not required
88.50215.99.19233.410.38263.512.13308.0Not required
1010.56268.211.31287.312.50317.514.25362.0Not required
1212.50317.513.38339.714.75374.716.63422.3Not required
1413.75349.314.63371.516.00406.419.13485.8Not required
1615.75400.116.63422.318.25463.621.25539.8Not required
1817.69449.318.69474.720.75527.123.50596.9Not required
2019.69500.120.69525.522.75577.925.75654.1Not required
2423.75603.324.75628.727.00685.830.50774.7Not required

Per ASME B16.20, checked against Lamons, Flexitallic and APG. Winding 0.175" (4.45 mm) thick; rings 0.117–0.131". breakingchips.com/gaskets/spiral-wound/class-300/

Thickness

Show
Winding
0.175" (4.45 mm), uncompressed
Inner and centering rings
0.117–0.131" (2.97–3.33 mm), nominally 1/8"

The rings stop the winding crushing: the joint is made up when the flanges close on them. Winding: Flexitallic and Wermac; ring range: Lamons and Wermac.

When the inner ring is required

Show
  • Class 900 NPS 24, Class 1500 NPS 12–24 and Class 2500 NPS 4–12.
  • Any PTFE-filled winding, at every size.
  • Flexitallic also fits one to every flexible graphite gasket unless the buyer says not to.

Elsewhere it is optional, though many makers fit one by default: it keeps the winding from buckling inward and smooths the flow past the joint. Lamons, Flexitallic and APG all print these rules.

Sources

Sources5