ASME B16.21 · non-metallic flat gaskets for ASME B16.5 flanges
Class 300 gasket dimensions
A Class 300 NPS 2 sheet gasket is 2.38" ID × 4.38" OD. Cut sizes for compressed fibre, PTFE, graphite and rubber sheet gaskets. A ring gasket sits inside the bolts on a raised face; a full-face gasket covers a flat-face flange out to its edge, with the bolt holes punched. Each size is checked against three or four published copies of the standard; a tag marks any that differ.
Class 300 sheet gasket chart
| NPS | ID (inmm) | Ring OD (inmm) | Full-face OD (inmm) | Holes | Hole Ø (inmm) | Bolt circle (inmm) |
|---|---|---|---|---|---|---|
| 1/2 | 0.8421.3 | 2.1253.8 | 3.7595.3 | 4 | 5/80.6316.0 | 2.6266.5 |
| 3/4 | 1.0626.9 | 2.6266.5 | 4.62117.3 | 4 | 3/40.7519.1 | 3.2582.6 |
| 1 | 1.3133.3 | 2.8873.2 | 4.88124.0 | 4 | 3/40.7519.1 | 3.5088.9 |
| 1-1/4 | 1.6642.2 | 3.2582.6 | 5.25133.4 | 4 | 3/40.7519.1 | 3.8898.6 |
| 1-1/2 | 1.9148.5 | 3.7595.3 | 6.12155.4 | 4 | 7/80.8822.4 | 4.50114.3 |
| 2 | 2.3860.5 | 4.38111.3 | 6.50165.1 | 8 | 3/40.7519.1 | 5.00127.0 |
| 2-1/2 | 2.8873.2 | 5.12130.0 | 7.50190.5 | 8 | 7/80.8822.4 | 5.88149.4 |
| 3 | 3.5088.9 | 5.88149.4 | 8.25209.6 | 8 | 7/80.8822.4 | 6.62168.1 |
| 3-1/2 | 4.00101.6 | 6.50165.1 | 9.00228.6 | 8 | 7/80.8822.4 | 7.25184.2 |
| 4 | 4.50114.3 | 7.12180.8 | 10.00254.0 | 8 | 7/80.8822.4 | 7.88200.2 |
| 5 | 5.56141.2 | 8.50215.9 | 11.00279.4 | 8 | 7/80.8822.4 | 9.25235.0 |
| 6 | 6.62168.1 | 9.88251.0 | 12.50317.5 | 12 | 7/80.8822.4 | 10.62269.7 |
| 8 | 8.62218.9 | 12.12307.8 | 15.00381.0 | 12 | 11.0025.4 | 13.00330.2 |
| 10 | 10.75273.1 | 14.25362.0 | 17.50444.5 | 16 | 1-1/81.1228.4 | 15.25387.4 |
| 12 | 12.75323.9 | 16.62422.1 | 20.50520.7 | 16 | 1-1/41.2531.8 | 17.75450.9 |
| 14 | 14.00355.6 | 19.12485.6 | 23.00584.2 | 20 | 1-1/41.2531.8 | 20.25514.4 |
| 16 | 16.00406.4 | 21.25539.8 | 25.50647.7 | 20 | 1-3/81.3835.1 | 22.50571.5 |
| 18 | 18.00457.2 | 23.50596.9 | 28.00711.2 | 24 | 1-3/81.3835.1 | 24.75628.7 |
| 20 | 20.00508.0 | 25.75654.1 | 30.50774.7 | 24 | 1-3/81.3835.1 | 27.00685.8 |
| 24 | 24.00609.6 | 30.50774.7 | 36.00914.4 | 24 | 1-5/81.6241.1 | 32.00812.8 |
Per ASME B16.21, checked against Garlock, Lamons, AmesWeb and Wermac. B16.21 sets the cut diameters, not the thickness. breakingchips.com/gaskets/sheet/class-300/
Before you cut
The ID, higher classes and full-face sizes
- The ID is the pipe’s outside diameter (0.84" at NPS 1/2), so it is the same in every class; the OD changes with the bolt circle.
- B16.21 lists no sheet gaskets above Class 900. For Class 1500 and 2500 use a spiral wound or ring joint gasket.
Other Class 300 gaskets
Sources
Sources6
The standard is ASME B16.21 — Nonmetallic Flat Gaskets for Pipe Flanges (archived Sep 10, 2026). Its sizes are checked against these copies, not averaged. Wermac prints whole millimetres; the millimetres shown here are inches × 25.4.
- Garlock — Ring and Full Face Gasket Dimensions, ASME B16.5 & B16.47 Series A & B, 150# through 2500# (archived Jul 18, 2026)
- Lamons — Gasket Handbook 2023: B16.21 ring and full-face gaskets (pp. 39–42), spiral wound WRI to B16.20 (pp. 72–77), ring joint (pp. 117–119) (archived Aug 12, 2025)
- AmesWeb — Flat ring nonmetallic gasket dimensions for Class 300, 400, 600 and 900 pipe flanges (archived Mar 14, 2026)
- Wermac — Dimensions of non-metallic flat ring gaskets, ASME B16.21, for B16.5 RF flanges (mm) (archived Oct 13, 2025)
- Wermac — Nonmetallic full face gaskets, Class 150 and 300, ASME B16.21 (mm) (archived Nov 14, 2025)