Mitsubishi · PVD-coated carbide

MP9015 insert grade

MP9015 is Mitsubishi’s PVD-coated carbide grade (PVD, High-Al (Al,Ti)N, single layer) for ISO S05–S25, as Mitsubishi’s catalog prints it. Heat resistant alloys, medium to rough cutting; the first recommendation for general work.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO S.cutting edgecoating PVDsubstrate carbideISO groupS
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Mitsubishi prints

Type
PVD-coated carbide
Coating
PVD, High-Al (Al,Ti)N, single layer
Substrate
Special carbide
ISO S
S05–S25 (core S15) · superalloys and titanium
Operations
turning

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

Mitsubishi’s first choice

  • Mitsubishi names MP9015 its first choice for Ni and Co-based alloys (e.g. Inconel 718), stable conditions: roughing.
  • Mitsubishi names MP9015 its first choice for Ni and Co-based alloys (e.g. Inconel 718), general conditions: finishing, medium and roughing.

One source: Mitsubishi Materials, its own catalog

Open the insert picker

MP9015 equivalents by material

ISO S (superalloys and titanium)

Read at S15, the centre of Mitsubishi’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC1008PVD-coated carbidePVD, AlTiN + TiNS10–S20

One source: ISCAR, its own catalog

KennametalKC5010PVD-coated carbidePVD, AlTiNS10–S20

One source: Kennametal, its own catalog

SandvikGC1105PVD-coated carbidePVDS05–S20 (core S15)

One source: Sandvik Coromant, its own catalog

SecoCP200PVD-coated carbidePVD, (Ti,Al)N + TiNabout S10–S20

One source: Seco Tools, its own catalog

Why MP9015 for heat-resistant superalloys (Inconel 718)

MP9015 for heat-resistant superalloys (Inconel 718): rated S05–S25 (core S15) by Mitsubishi.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    Mitsubishi rates MP9015 (PVD-coated carbide) for S05–S25 (core S15): Heat resistant alloys, medium to rough cutting; the first recommendation for general work.

    One source: Mitsubishi Materials, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a compilation across makers, lists MP9015 at S10, S20. Mitsubishi Materials’ own catalog is the authority for its grade.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)