Sandvik · PVD-coated carbide
GC1105 insert grade
GC1105 is Sandvik’s PVD-coated carbide grade (PVD) for ISO S05–S20, as Sandvik’s catalog prints it. Heat resistant superalloys, finishing to medium machining.
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Type
- PVD-coated carbide
- Coating
- PVD
- ISO S
- S05–S20 (core S15) · superalloys and titanium
- Operations
- turning
Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
GC1105 equivalents by material
ISO S (superalloys and titanium)
Read at S15, the centre of Sandvik’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1008 | PVD-coated carbide | PVD, AlTiN + TiN | S10–S20 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Seco | CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about S10–S20 | One source: Seco Tools, its own catalog |
Why GC1105 for heat-resistant superalloys (Inconel 718)
GC1105 for heat-resistant superalloys (Inconel 718): rated S05–S20 (core S15) by Sandvik.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Sandvik rates GC1105 (PVD-coated carbide) for S05–S20 (core S15): Heat resistant superalloys, finishing to medium machining.
One source: Sandvik Coromant, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC1105 at M10, S10. Sandvik Coromant’s own catalog is the authority for its grade.
- The cross-reference lists M10; Sandvik Coromant gives no M application (its range: S05–S20).
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)