Insert grades · Mitsubishi

Mitsubishi insert grade chart

28 Mitsubishi insert grades, each as Mitsubishi’s own catalog prints it: 11 CVD-coated carbide, 9 PVD-coated carbide, 3 cermet, 4 uncoated carbide and 1 micro-grain carbide. The table gives each grade’s coating and ISO range; each page lists the other makers’ grades for the same class.

One source: Mitsubishi Materials, its own catalog

The six ISO groups, with how many of the maker’s listed grades cover each: P 10, M 11, K 12, N 1, S 9, H none.PMKNSH101112190
Mitsubishi’s listed grades by ISO group.

Mitsubishi insert grades by type

Mitsubishi insert grades: type, coating and ISO range
GradeTypeCoatingISO range
MC5005CVD-coated carbideCVDK01–K20
MC5015CVD-coated carbideCVDK05–K25
MC5105CVD-coated carbideCVD, TiCN-Al2O3, thickK01–K20
MC5115CVD-coated carbideCVD, TiCN-Al2O3, thickK05–K25
MC6115CVD-coated carbideCVD, Accumulated TiCN-Al2O3-Ti compound, thickP01–P25
MC6125CVD-coated carbideCVD, Accumulated TiCN-Al2O3-Ti compound, thickP10–P35
MC7015CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM05–M25
MC7025CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM20–M40
US735CVD-coated carbideCVD, Ti compound, thinM30–M50
US905CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinS01–S10
US7020CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM10–M30
MP9005PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS01–S20
MP9015PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS05–S25
MP9025PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS15–S35
MS6015PVD-coated carbidePVDP10–P30
VP05RTPVD-coated carbidePVDS01–S20
VP10RTPVD-coated carbidePVDP10–P30, M10–M30, K10–K30 and S05–S25
VP15TFPVD-coated carbidePVDP20–P40, M20–M40 and K20–K40
VP20MFPVD-coated carbidePVDP20–P40 and M20–M40
VP20RTPVD-coated carbidePVDM20–M40, K20–K40 and S15–S35
AP25NcermetPVDP05–P25, M05–M25 and K05–K25
MP3025cermetPVD, Ti compoundP15–P35
NX2525cermetUncoatedP10–P25, M10–M25 and K10–K25
HTi10uncoated carbideUncoatedK10–K20 and N10–N20
MT9005uncoated carbideUncoatedS01–S20
MT9015uncoated carbideUncoatedS05–S25
UTi20Tuncoated carbideUncoatedP25–P40, M25–M40 and K20–K35
TF15micro-grain carbideUncoatedK20–K20
Sources1