Insert grades · Sandvik

Sandvik insert grade chart

15 Sandvik insert grades, each as Sandvik’s own catalog prints it: 8 CVD-coated carbide, 4 PVD-coated carbide, 1 cermet and 2 uncoated carbide. The table gives each grade’s coating and ISO range; each page lists the other makers’ grades for the same class.

One source: Sandvik Coromant, its own catalog

The six ISO groups, with how many of the maker’s listed grades cover each: P 5, M 6, K 1, N 2, S 5, H none.PMKNSH561250
Sandvik’s listed grades by ISO group.

Sandvik insert grades by type

Sandvik insert grades: type, coating and ISO range
GradeTypeCoatingISO range
GC2015CVD-coated carbideCVDM05–M25
GC2025CVD-coated carbideCVDM15–M35
GC2220CVD-coated carbideCoated (process not printed)M15–M30
GC4305CVD-coated carbideCVDP01–P15
GC4315CVD-coated carbideCVDP01–P30
GC4325CVD-coated carbideCVDP10–P40
GC4335CVD-coated carbideCVDP25–P45
S05FCVD-coated carbideCVDS05–S15
GC1105PVD-coated carbidePVDS05–S20
GC1115PVD-coated carbidePVDM05–M25 and S15–S25
GC1125PVD-coated carbidePVDM10–M30 and S20–S30
GC2035PVD-coated carbidePVDM25–M40
GC1525cermetPVDP05–P25
H10uncoated carbideUncoatedN01–N25
H13Auncoated carbideUncoatedK10–K30, N05–N25 and S10–S30
Sources1