Sandvik · CVD-coated carbide
GC4305 insert grade
GC4305 is Sandvik’s CVD-coated carbide grade (CVD) for ISO P01–P15, as Sandvik’s catalog prints it. Steel in stable conditions where a higher metal removal rate is needed, medium to rough; withstands high temperatures.
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Type
- CVD-coated carbide
- Coating
- CVD
- ISO P
- P01–P15 (core P05) · steel
- Operations
- turning
Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
GC4305 equivalents by material
ISO P (steel)
Read at P05, the centre of Sandvik’s P range (steel). Each grade is one its own maker rates for P05 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Mitsubishi | MC6115 | CVD-coated carbide | CVD, Accumulated TiCN-Al2O3-Ti compound, thick | P01–P25 (core P10) | One source: Mitsubishi Materials, its own catalog |
Why GC4305 for steel
GC4305 for steel: rated P01–P15 (core P05) by Sandvik.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
Sandvik rates GC4305 (CVD-coated carbide) for P01–P15 (core P05): Steel in stable conditions where a higher metal removal rate is needed, medium to rough; withstands high temperatures.
One source: Sandvik Coromant, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC4305 at P01. Sandvik Coromant’s own catalog is the authority for its grade.
It agrees with Sandvik Coromant’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)