Mitsubishi · CVD-coated carbide
MC6115 insert grade
MC6115 is Mitsubishi’s CVD-coated carbide grade (CVD, Accumulated TiCN-Al2O3-Ti compound, thick) for ISO P01–P25, as Mitsubishi’s catalog prints it. Steel, continuous cutting; wear resistance at high temperature.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- CVD-coated carbide
- Coating
- CVD, Accumulated TiCN-Al2O3-Ti compound, thick
- Substrate
- 90.8 HRA
- ISO P
- P01–P25 (core P10) · steel
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Mitsubishi’s first choice
- Mitsubishi names MC6115 its first choice for carbon and alloy steel, 180–280 HB (e.g. 1045, 4140), stable conditions: medium and roughing.
One source: Mitsubishi Materials, its own catalog
Open the insert pickerMC6115 equivalents by material
ISO P (steel)
Read at P10, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC8250 | CVD-coated carbide | CVD, TiCN + Al2O3 + TiN | P10–P35 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | P10–P20 | One source: Kennametal, its own catalog |
| Sandvik | GC4305 | CVD-coated carbide | CVD | P01–P15 (core P05) | One source: Sandvik Coromant, its own catalog |
| Seco | TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | about P10–P20 | One source: Seco Tools, its own catalog |
Why MC6115 for steel
MC6115 for steel: rated P01–P25 (core P10) by Mitsubishi.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
Mitsubishi rates MC6115 (CVD-coated carbide) for P01–P25 (core P10): Steel, continuous cutting; wear resistance at high temperature.
One source: Mitsubishi Materials, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)