Seco · PVD-coated carbide

TS2050 insert grade

TS2050 is Seco’s PVD-coated carbide grade (PVD, Ti-Al-Si-N nanolaminate) for ISO S05–S15, as Seco’s catalog prints it. Finishing and semi-finishing superalloys.

One source: Seco Tools, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO S.cutting edgecoating PVDsubstrate carbideISO groupS
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Seco prints

Type
PVD-coated carbide
Coating
PVD, Ti-Al-Si-N nanolaminate
Substrate
Hard, wear-resistant micrograin
ISO S
about S05–S15 · superalloys and titanium
Secondary
ISO M, H (Seco names them in its text only)
Operations
turning

Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.

Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)

TS2050 equivalents by material

ISO S (superalloys and titanium)

Read at S10, the centre of Seco’s S range (superalloys and titanium). Each grade is one its own maker rates for S10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S10
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC804PVD-coated carbidePVD, AlTiN (SUMOTEC treated)S05–S15

One source: ISCAR, its own catalog

KennametalKC5010PVD-coated carbidePVD, AlTiNS10–S20

One source: Kennametal, its own catalog

MitsubishiMP9005PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS01–S20 (core S10)

One source: Mitsubishi Materials, its own catalog

SandvikGC1105PVD-coated carbidePVDS05–S20 (core S15)

One source: Sandvik Coromant, its own catalog

Why TS2050 for heat-resistant superalloys (Inconel 718)

TS2050 for heat-resistant superalloys (Inconel 718): rated about S05–S15 by Seco.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    Seco rates TS2050 (PVD-coated carbide) for about S05–S15: Finishing and semi-finishing superalloys.

    One source: Seco Tools, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists TS2050 at S10. Seco Tools’ own catalog is the authority for its grade.

It agrees with Seco Tools’ catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)