Insert grades · Seco
Seco insert grade chart
15 Seco insert grades, each as Seco’s own catalog prints it: 4 CVD-coated carbide, 7 PVD-coated carbide, 1 cermet, 1 uncoated carbide and 2 micro-grain carbide. The table gives each grade’s coating and ISO range; each page lists the other makers’ grades for the same class.
One source: Seco Tools, its own catalog
Seco insert grades by type
| Grade | Type | Coating | ISO range |
|---|---|---|---|
| TM1501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | M10–M20 |
| TM2501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | M20–M25 |
| TM3501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | M25–M35 |
| TS0501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | S01–S05 |
| CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | M01–M10 and S10–S20 |
| CP500 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | M10–M30 |
| CP600 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | M20–M40 |
| TH1000 | PVD-coated carbide | PVD, Ti-Al-Si-N nanolaminate | S01–S10 and H05–H15 |
| TS2000 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | M01–M10 and S05–S20 |
| TS2050 | PVD-coated carbide | PVD, Ti-Al-Si-N nanolaminate | S05–S15 |
| TS2500 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | S10–S20 |
| TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | P10–P20 |
| HX | uncoated carbide | Uncoated | S10–S25 |
| 883 | micro-grain carbide | Uncoated | S10–S30 |
| 890 | micro-grain carbide | Uncoated | S10–S20 |