27 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 27 HRC equals 279 HV (Vickers) and 264 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

27 HRC on the three scales: 264 HB and 279 HV, as ASTM E140 converts it.HRCHBHVHRC 27HB 264HV 2792025404550556065400500600700300400500600700900
27 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
264 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
279 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 24 to 30 in Vickers and Brinell
HRCHVHB
24 HRC260247
25 HRC266253
26 HRC272258
27 HRC279264
28 HRC286271
29 HRC294279
30 HRC302286