ASTM E140 · Non-austenitic steel

28 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 28 HRC equals 286 HV (Vickers) and 271 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

28 HRC on the three scales: 271 HB and 286 HV, as ASTM E140 converts it.HRCHBHVHRC 28HB 271HV 2862025404550556065400500600700400500600700900
28 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
271 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
286 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 25 to 31 in Vickers and Brinell
HRCHVHB
25 HRC266253
26 HRC272258
27 HRC279264
28 HRC286271
29 HRC294279
30 HRC302286
31 HRC310294

Sources

Sources5