ASTM E140 · Non-austenitic steel

29 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 29 HRC equals 294 HV (Vickers) and 279 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

29 HRC on the three scales: 279 HB and 294 HV, as ASTM E140 converts it.HRCHBHVHRC 29HB 279HV 2942025404550556065400500600700400500600700900
29 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
279 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
294 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 26 to 32 in Vickers and Brinell
HRCHVHB
26 HRC272258
27 HRC279264
28 HRC286271
29 HRC294279
30 HRC302286
31 HRC310294
32 HRC318301

Sources

Sources5