ASTM E140 · Non-austenitic steel

40 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 40 HRC equals 392 HV (Vickers) and 371 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

40 HRC on the three scales: 371 HB and 392 HV, as ASTM E140 converts it.HRCHBHVHRC 40HB 371HV 3922025303550556065300500600700300500600700900
40 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
371 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
392 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 37 to 43 in Vickers and Brinell
HRCHVHB
37 HRC363344
38 HRC372353
39 HRC382362
40 HRC392371
41 HRC402381
42 HRC412390
43 HRC423400

Sources

Sources5