ASTM E140 · Non-austenitic steel

41 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 41 HRC equals 402 HV (Vickers) and 381 HB (Brinell, 10 mm carbide ball), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

41 HRC on the three scales: 381 HB and 402 HV, as ASTM E140 converts it.HRCHBHVHRC 41HB 381HV 40220253035556065300500600700300500600700900
41 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
381 HB

10 mm carbide ball, 3000 kgf (HBW)

Vickers
402 HV

Checked against 5 published copies

Nearby values

Other sizes
Rockwell C 38 to 44 in Vickers and Brinell
HRCHVHB
38 HRC372353
39 HRC382362
40 HRC392371
41 HRC402381
42 HRC412390
43 HRC423400
44 HRC434409

Sources

Sources5