61 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 61 HRC equals 720 HV (Vickers) and 670 HB (Brinell, 10 mm carbide ball; E140 prints it in parentheses, above Brinell’s 650 limit), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

61 HRC on the three scales: (670) HB and 720 HV, as ASTM E140 converts it.HRCHBHVHRC 61HB (670)HV 72020253035404565300400500300400500600900
61 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
(670) HB

10 mm carbide ball, 3000 kgf (HBW). In parentheses: above 650, past Brinell’s recommended range

Vickers
720 HV

Checked against 4 published copies

Nearby values

Other sizes
Rockwell C 58 to 64 in Vickers and Brinell
HRCHVHB
58 HRC653615
59 HRC674634
60 HRC697(654)
61 HRC720(670)
62 HRC746(688)
63 HRC772(705)
64 HRC800(722)