ASTM E140 · Non-austenitic steel

62 HRC to HV and HB (ASTM E140)

By ASTM E140 Table 1, 62 HRC equals 746 HV (Vickers) and 688 HB (Brinell, 10 mm carbide ball; E140 prints it in parentheses, above Brinell’s 650 limit), for carbon, alloy and tool steel. Conversions are approximate; austenitic stainless, cast iron and nonferrous metals need other tables.

62 HRC on the three scales: (688) HB and 746 HV, as ASTM E140 converts it.HRCHBHVHRC 62HB (688)HV 7462025303540455065300400500300400500600900
62 HRC across the ASTM E140 scales. The scales aligned by E140’s conversion rows; they are not linear against each other.
Brinell
(688) HB

10 mm carbide ball, 3000 kgf (HBW). In parentheses: above 650, past Brinell’s recommended range

Vickers
746 HV

Checked against 4 published copies

Nearby values

Other sizes
Rockwell C 59 to 65 in Vickers and Brinell
HRCHVHB
59 HRC674634
60 HRC697(654)
61 HRC720(670)
62 HRC746(688)
63 HRC772(705)
64 HRC800(722)
65 HRC832(739)

Sources

Sources5