Pipe schedule chart

1-1/4" pipe schedule

NPS 1-1/4 (DN 32) pipe is 1.660" outside diameter in every schedule. Schedule 40 has a 0.140" wall and a 1.380" ID; Schedule 80 has a 0.191" wall and a 1.278" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 1.66" OD, in Schedule 40 and Schedule 80: the same OD, the wall setting the bore.OD 1.66"schedule 40ID 1.380"wall 0.140"schedule 80ID 1.278"wall 0.191"
1.66" OD pipe in Schedule 40 and Schedule 80. Each ring drawn to scale; the two to the same scale.

Outside diameter

1.660"42.16 mm

NPS 1-1/4 · DN 32

Checked against 5 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

1-1/4" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
5S0.0651.651.53038.861.111.650.3262.101.83911.86Checked against 4 published copies
Sch 10 · 10S0.1092.771.44236.631.812.690.5313.431.63310.54Checked against 3 published copies
STD · Sch 40 · 40S0.1403.561.38035.052.273.390.6694.311.4969.65Checked against 4 published copies
XS · Sch 80 · 80S0.1914.851.27832.463.004.460.8815.691.2838.28Checked against 4 published copies
Sch 1600.2506.351.16029.463.775.611.1077.141.0576.82Checked against 4 published copies
XXS0.3829.700.89622.765.227.771.5349.890.6314.07Checked against 4 published copies

Checked against 3 published copies

Notes for 1-1/4" pipe

STD and XS, stainless, weight and what's not shown
  • STD and Sch 40 are the same wall here (0.140"). They part above NPS 10.
  • XS and Sch 80 are the same wall here (0.191"). They part above NPS 8.
  • Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 1.660").