1-1/2" pipe schedule
NPS 1-1/2 (DN 40) pipe is 1.900" outside diameter in every schedule. Schedule 40 has a 0.145" wall and a 1.610" ID; Schedule 80 has a 0.200" wall and a 1.500" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
1.900"48.26 mm
NPS 1-1/2 · DN 40
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.0651.65 | 1.77044.96 | 1.281.90 | 0.3752.42 | 2.46115.87 | Checked against 4 published copies |
| Sch 10 · 10S | 0.1092.77 | 1.68242.72 | 2.093.11 | 0.6133.96 | 2.22214.34 | Checked against 3 published copies |
| STD · Sch 40 · 40S | 0.1453.68 | 1.61040.89 | 2.724.05 | 0.7995.16 | 2.03613.13 | Checked against 4 published copies |
| XS · Sch 80 · 80S | 0.2005.08 | 1.50038.10 | 3.635.41 | 1.0686.89 | 1.76711.40 | Checked against 4 published copies |
| Sch 160 | 0.2817.14 | 1.33833.99 | 4.867.24 | 1.4299.22 | 1.4069.07 | Checked against 4 published copies |
| XXS | 0.40010.16 | 1.10027.94 | 6.419.55 | 1.88512.16 | 0.9506.13 | Checked against 4 published copies |
Checked against 3 published copies
Notes for 1-1/2" pipe
STD and XS, stainless, weight and what's not shown
- STD and Sch 40 are the same wall here (0.145"). They part above NPS 10.
- XS and Sch 80 are the same wall here (0.200"). They part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 1.900").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)