Pipe schedule chart
12" pipe schedule
NPS 12 (DN 300) pipe is 12.750" outside diameter in every schedule. Schedule 40 has a 0.406" wall and a 11.938" ID; Schedule 80 has a 0.688" wall and a 11.374" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
12.750"323.85 mm
NPS 12 · DN 300
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.1563.96 | 12.438315.93 | 21.0031.25 | 6.17239.82 | 121.504783.90 | Checked against 3 published copies |
| Sch 10 · 10S | 0.1804.57 | 12.390314.71 | 24.1935.99 | 7.10845.86 | 120.568777.86 | Two published copies agree |
| Sch 20 | 0.2506.35 | 12.250311.15 | 33.4149.71 | 9.81763.34 | 117.859760.38 | Checked against 4 published copies |
| Sch 30 | 0.3308.38 | 12.090307.09 | 43.8165.20 | 12.87683.07 | 114.800740.64 | Checked against 4 published copies |
| STD · 40S | 0.3759.53 | 12.000304.80 | 49.6173.83 | 14.57994.06 | 113.097729.66 | Checked against 4 published copies |
| Sch 40 | 0.40610.31 | 11.938303.23 | 53.5779.73 | 15.745101.58 | 111.932722.14 | Checked against 5 published copies |
| XS · 80S | 0.50012.70 | 11.750298.45 | 65.4897.44 | 19.242124.14 | 108.434699.57 | Checked against 4 published copies |
| Sch 60 | 0.56214.27 | 11.626295.30 | 73.22108.97 | 21.519138.83 | 106.157684.89 | Checked against 4 published copies |
| Sch 80 | 0.68817.48 | 11.374288.90 | 88.71132.02 | 26.071168.20 | 101.605655.52 | Checked against 5 published copies |
| Sch 100 | 0.84421.44 | 11.062280.97 | 107.42159.86 | 31.569203.67 | 96.107620.05 | Checked against 4 published copies |
| Sch 120 | 1.00025.40 | 10.750273.05 | 125.61186.92 | 36.914238.15 | 90.763585.56 | Checked against 4 published copies |
| Sch 140 | 1.12528.58 | 10.500266.70 | 139.81208.05 | 41.086265.07 | 86.590558.64 | Checked against 4 published copies |
| Sch 160 | 1.31233.32 | 10.126257.20 | 160.42238.73 | 47.145304.16 | 80.531519.56 | Checked against 4 published copies |
Two published copies agree
- 5S: Guanyu Tube (TubingChina) prints 0.165"; the other copies print 0.156".
Notes for 12" pipe
STD and XS, stainless, weight and what's not shown
- STD (0.375") is not Sch 40 (0.406") at this size: they part above NPS 10.
- XS (0.500") is not Sch 80 (0.688") at this size: they part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 12.750").
- Not shown: XXS (only Project Materials prints it, 1.000").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina), Metal Supermarkets.