Pipe schedule chart

10" pipe schedule

NPS 10 (DN 250) pipe is 10.750" outside diameter in every schedule. Schedule 40 has a 0.365" wall and a 10.020" ID; Schedule 80 has a 0.594" wall and a 9.562" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 10.75" OD, in Schedule 40 and Schedule 80: the same OD, the wall setting the bore.OD 10.75"schedule 40ID 10.020"wall 0.365"schedule 80ID 9.562"wall 0.594"
10.75" OD pipe in Schedule 40 and Schedule 80. Each ring drawn to scale; the two to the same scale.

Outside diameter

10.750"273.05 mm

NPS 10 · DN 250

Checked against 5 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

10" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
5S0.1343.4010.482266.2415.2122.634.46928.8386.294556.73Checked against 4 published copies
Sch 10 · 10S0.1654.1910.420264.6718.6727.785.48735.4085.276550.16Two published copies agree
Sch 200.2506.3510.250260.3528.0641.768.24753.2082.516532.36Checked against 4 published copies
Sch 300.3077.8010.136257.4534.2751.0010.07264.9880.691520.58Checked against 4 published copies
STD · Sch 40 · 40S0.3659.2710.020254.5140.5260.3011.90876.8378.854508.74Checked against 4 published copies
Sch 60 · XS · 80S0.50012.709.750247.6554.7981.5316.101103.8874.662481.69Checked against 4 published copies
Sch 800.59415.099.562242.8764.4995.9718.952122.2771.810463.29Checked against 5 published copies
Sch 1000.71918.269.312236.5277.10114.7422.658146.1868.105439.38Checked against 4 published copies
Sch 1200.84421.449.062230.1789.38133.0126.266169.4664.497416.11Checked against 4 published copies
Sch 1401.00025.408.750222.25104.23155.1130.631197.6260.132387.95Checked against 4 published copies
Sch 1601.12528.588.500215.90115.75172.2634.018219.4756.745366.10Checked against 4 published copies

Two published copies agree

Notes for 10" pipe

STD and XS, stainless, weight and what's not shown
  • STD and Sch 40 are the same wall here (0.365"). They part above NPS 10.
  • XS (0.500") is not Sch 80 (0.594") at this size: they part above NPS 8.
  • Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 10.750").
  • Not shown: XXS (only Project Materials prints it, 1.000").