16" pipe schedule
NPS 16 (DN 400) pipe is 16.000" outside diameter in every schedule. Schedule 40 has a 0.500" wall and a 15.000" ID; Schedule 80 has a 0.844" wall and a 14.312" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
16.000"406.40 mm
NPS 16 · DN 400
Checked against 4 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.1654.19 | 15.670398.02 | 27.9341.57 | 8.20852.96 | 192.8541,244.21 | Two published copies agree |
| 10S | 0.1884.78 | 15.624396.85 | 31.7847.29 | 9.33960.25 | 191.7231,236.92 | Checked against 3 published copies |
| Sch 10 | 0.2506.35 | 15.500393.70 | 42.0962.64 | 12.37079.81 | 188.6921,217.36 | Checked against 4 published copies |
| Sch 20 | 0.3127.92 | 15.376390.55 | 52.3277.87 | 15.37799.21 | 185.6851,197.96 | Checked against 4 published copies |
| Sch 30 · STD · 40S | 0.3759.53 | 15.250387.35 | 62.6493.21 | 18.408118.76 | 182.6541,178.41 | Two published copies agree |
| Sch 40 · XS · 80S | 0.50012.70 | 15.000381.00 | 82.85123.29 | 24.347157.08 | 176.7151,140.09 | Two published copies agree |
| Sch 60 | 0.65616.66 | 14.688373.08 | 107.60160.13 | 31.622204.01 | 169.4401,093.16 | Checked against 4 published copies |
| Sch 80 | 0.84421.44 | 14.312363.52 | 136.74203.50 | 40.186259.27 | 160.8761,037.91 | Checked against 4 published copies |
| Sch 100 | 1.03126.19 | 13.938354.03 | 164.98245.52 | 48.484312.80 | 152.578984.37 | Checked against 4 published copies |
| Sch 120 | 1.21930.96 | 13.562344.47 | 192.61286.64 | 56.605365.20 | 144.457931.98 | Checked against 4 published copies |
| Sch 140 | 1.43836.53 | 13.124333.35 | 223.85333.13 | 65.785424.42 | 135.276872.75 | Checked against 4 published copies |
| Sch 160 | 1.59440.49 | 12.812325.42 | 245.48365.31 | 72.141465.42 | 128.921831.75 | Checked against 4 published copies |
Two published copies agree
Notes for 16" pipe
STD and XS, stainless, weight and what's not shown
- STD (0.375") is not Sch 40 (0.500") at this size: they part above NPS 10.
- XS (0.500") is not Sch 80 (0.844") at this size: they part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 16.000").
Sources
Sources7
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina).