Pipe schedule chart
18" pipe schedule
NPS 18 (DN 450) pipe is 18.000" outside diameter in every schedule. Schedule 40 has a 0.562" wall and a 16.876" ID; Schedule 80 has a 0.938" wall and a 16.124" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
18.000"457.20 mm
NPS 18 · DN 450
Checked against 4 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.1654.19 | 17.670448.82 | 31.4646.82 | 9.24559.65 | 245.2241,582.09 | Two published copies agree |
| 10S | 0.1884.78 | 17.624447.65 | 35.8053.27 | 10.52067.87 | 243.9491,573.86 | Checked against 3 published copies |
| Sch 10 | 0.2506.35 | 17.500444.50 | 47.4470.59 | 13.94189.94 | 240.5281,551.79 | Checked against 4 published copies |
| Sch 20 | 0.3127.92 | 17.376441.35 | 58.9987.79 | 17.337111.85 | 237.1321,529.88 | Checked against 4 published copies |
| STD · 40S | 0.3759.53 | 17.250438.15 | 70.65105.15 | 20.764133.96 | 233.7051,507.77 | Two published copies agree |
| Sch 30 | 0.43811.13 | 17.124434.95 | 82.23122.37 | 24.166155.91 | 230.3031,485.83 | Checked against 4 published copies |
| XS · 80S | 0.50012.70 | 17.000431.80 | 93.54139.20 | 27.489177.35 | 226.9801,464.38 | Two published copies agree |
| Sch 40 | 0.56214.27 | 16.876428.65 | 104.76155.91 | 30.788198.63 | 223.6811,443.10 | Checked against 4 published copies |
| Sch 60 | 0.75019.05 | 16.500419.10 | 138.30205.82 | 40.644262.22 | 213.8251,379.51 | Checked against 4 published copies |
| Sch 80 | 0.93823.83 | 16.124409.55 | 171.08254.60 | 50.279324.38 | 204.1901,317.36 | Checked against 4 published copies |
| Sch 100 | 1.15629.36 | 15.688398.48 | 208.15309.76 | 61.172394.66 | 193.2971,247.07 | Checked against 4 published copies |
| Sch 120 | 1.37534.93 | 15.250387.35 | 244.37363.66 | 71.815463.32 | 182.6541,178.41 | Checked against 4 published copies |
| Sch 140 | 1.56239.67 | 14.876377.85 | 274.48408.47 | 80.664520.41 | 173.8051,121.32 | Checked against 4 published copies |
| Sch 160 | 1.78145.24 | 14.438366.73 | 308.79459.53 | 90.748585.47 | 163.7211,056.26 | Checked against 4 published copies |
Two published copies agree
Notes for 18" pipe
STD and XS, stainless, weight and what's not shown
- STD (0.375") is not Sch 40 (0.562") at this size: they part above NPS 10.
- XS (0.500") is not Sch 80 (0.938") at this size: they part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 18.000").
Sources
Sources7
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina).