Pipe schedule chart
24" pipe schedule
NPS 24 (DN 600) pipe is 24.000" outside diameter in every schedule. Schedule 40 has a 0.688" wall and a 22.624" ID; Schedule 80 has a 1.219" wall and a 21.562" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
24.000"609.60 mm
NPS 24 · DN 600
Checked against 4 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.2185.54 | 23.564598.53 | 55.4282.48 | 16.288105.08 | 436.1022,813.55 | Two published copies agree |
| Sch 10 · 10S | 0.2506.35 | 23.500596.90 | 63.4794.46 | 18.653120.34 | 433.7362,798.29 | Two published copies agree |
| Sch 20 · STD · 40S | 0.3759.53 | 23.250590.55 | 94.71140.94 | 27.833179.56 | 424.5572,739.07 | Two published copies agree |
| XS · 80S | 0.50012.70 | 23.000584.20 | 125.61186.92 | 36.914238.15 | 415.4762,680.48 | Two published copies agree |
| Sch 30 | 0.56214.27 | 22.876581.05 | 140.81209.55 | 41.382266.98 | 411.0082,651.66 | Checked against 3 published copies |
| Sch 40 | 0.68817.48 | 22.624574.65 | 171.45255.15 | 50.387325.08 | 402.0022,593.56 | Checked against 3 published copies |
| Sch 60 | 0.96924.61 | 22.062560.37 | 238.57355.03 | 70.111452.33 | 382.2782,466.31 | Checked against 3 published copies |
| Sch 80 | 1.21930.96 | 21.562547.67 | 296.86441.78 | 87.242562.85 | 365.1472,355.78 | Checked against 3 published copies |
| Sch 100 | 1.53138.89 | 20.938531.83 | 367.74547.25 | 108.071697.23 | 344.3182,221.40 | Checked against 3 published copies |
| Sch 120 | 1.81246.02 | 20.376517.55 | 429.79639.59 | 126.307814.88 | 326.0832,103.76 | Checked against 3 published copies |
| Sch 140 | 2.06252.37 | 19.876504.85 | 483.57719.64 | 142.114916.86 | 310.2762,001.78 | Checked against 3 published copies |
| Sch 160 | 2.34459.54 | 19.312490.52 | 542.64807.54 | 159.4721,028.85 | 292.9171,889.78 | Checked against 3 published copies |
Two published copies agree
Notes for 24" pipe
STD and XS, stainless, weight and what's not shown
- STD (0.375") is not Sch 40 (0.688") at this size: they part above NPS 10.
- XS (0.500") is not Sch 80 (1.219") at this size: they part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 24.000").
Sources
Sources9
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Wikipedia, Nominal Pipe Size: wall thickness tables (used only for the large-pipe cells no other copy prints; to be replaced) (archived Nov 9, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
- Project Materials, What is ASME B36.19? (scope NPS 1/8 to 30) (archived Apr 22, 2026)
- HT Pipe, ASME B36.19 (40S and 80S stop at NPS 24; 22 and 30 are 5S and 10S only) (archived Jul 12, 2026)
Copies of B36.10M / B36.19M that print this size: Wikipedia, Engineers Edge, Project Materials, Guanyu Tube (TubingChina).