Pipe schedule chart

22" pipe schedule

NPS 22 (DN 550) pipe is 22.000" outside diameter in every schedule. STD has a 0.375" wall and a 21.250" ID; Schedule 80 has a 1.125" wall and a 19.750" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 22" OD, in STD and Schedule 80: the same OD, the wall setting the bore.OD 22"schedule STDID 21.250"wall 0.375"schedule 80ID 19.750"wall 1.125"
22" OD pipe in STD and Schedule 80. Each ring drawn to scale; the two to the same scale.

Outside diameter

22.000"558.80 mm

NPS 22 · DN 550

Checked against 3 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

22" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
Sch 100.2506.3521.500546.1058.1386.5017.082110.21363.0502,342.26Two published copies agree
Sch 20 · STD0.3759.5321.250539.7586.69129.0125.476164.36354.6562,288.10Two published copies agree
Sch 30 · XS0.50012.7021.000533.40114.92171.0233.772217.88346.3612,234.58Two published copies agree
Sch 600.87522.2320.250514.35197.60294.0658.070374.65322.0622,077.82Two published copies agree
Sch 801.12528.5819.750501.65251.05373.6073.778475.99306.3541,976.48Two published copies agree
Sch 1001.37534.9319.250488.95303.16451.1589.094574.80291.0391,877.67Two published copies agree
Sch 1201.62541.2818.750476.25353.94526.72104.016671.07276.1171,781.39Two published copies agree
Sch 1401.87547.6318.250463.55403.38600.30118.546764.81261.5871,687.65Two published copies agree
Sch 1602.12553.9817.750450.85451.49671.88132.683856.02247.4501,596.45Two published copies agree

Published copies disagree: Wikipedia 0.218"; Guanyu Tube (TubingChina) 0.25"

10S: not shown as one number.

Published copies disagree: Wikipedia 0.218"; Guanyu Tube (TubingChina) 0.25"

Notes for 22" pipe

STD and XS, stainless, weight and what's not shown
  • XS (0.500") is not Sch 80 (1.125") at this size: they part above NPS 8.
  • Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 22.000").
  • Not shown: 40S (B36.19M lists none at this size; Guanyu Tube (TubingChina) print STD/XS under it); 80S (B36.19M lists none at this size; Guanyu Tube (TubingChina) print STD/XS under it).