Pipe schedule chart

3" pipe schedule

NPS 3 (DN 80) pipe is 3.500" outside diameter in every schedule. Schedule 40 has a 0.216" wall and a 3.068" ID; Schedule 80 has a 0.300" wall and a 2.900" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 3.5" OD, in Schedule 40 and Schedule 80: the same OD, the wall setting the bore.OD 3.5"schedule 40ID 3.068"wall 0.216"schedule 80ID 2.900"wall 0.300"
3.5" OD pipe in Schedule 40 and Schedule 80. Each ring drawn to scale; the two to the same scale.

Outside diameter

3.500"88.90 mm

NPS 3 · DN 80

Checked against 5 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

3" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
5S0.0832.113.33484.683.034.510.8915.758.73056.32Checked against 4 published copies
Sch 10 · 10S0.1203.053.26082.804.346.451.2748.228.34753.85Checked against 3 published copies
STD · Sch 40 · 40S0.2165.493.06877.937.5811.282.22814.387.39347.69Checked against 4 published copies
XS · Sch 80 · 80S0.3007.622.90073.6610.2615.273.01619.466.60542.61Checked against 4 published copies
Sch 1600.43811.132.62466.6514.3421.344.21327.185.40834.89Checked against 4 published copies
XXS0.60015.242.30058.4218.6027.685.46635.274.15526.80Checked against 4 published copies

Checked against 3 published copies

Notes for 3" pipe

STD and XS, stainless, weight and what's not shown
  • STD and Sch 40 are the same wall here (0.216"). They part above NPS 10.
  • XS and Sch 80 are the same wall here (0.300"). They part above NPS 8.
  • Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 3.500").

Sources

Sources8