Pipe schedule chart
2-1/2" pipe schedule
NPS 2-1/2 (DN 65) pipe is 2.875" outside diameter in every schedule. Schedule 40 has a 0.203" wall and a 2.469" ID; Schedule 80 has a 0.276" wall and a 2.323" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
2.875"73.03 mm
NPS 2-1/2 · DN 65
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.0832.11 | 2.70968.81 | 2.483.69 | 0.7284.70 | 5.76437.19 | Checked against 4 published copies |
| Sch 10 · 10S | 0.1203.05 | 2.63566.93 | 3.535.26 | 1.0396.70 | 5.45335.18 | Checked against 3 published copies |
| STD · Sch 40 · 40S | 0.2035.16 | 2.46962.71 | 5.808.63 | 1.70410.99 | 4.78830.89 | Checked against 4 published copies |
| XS · Sch 80 · 80S | 0.2767.01 | 2.32359.00 | 7.6711.41 | 2.25414.54 | 4.23827.34 | Checked against 4 published copies |
| Sch 160 | 0.3759.53 | 2.12553.98 | 10.0214.91 | 2.94519.00 | 3.54722.88 | Checked against 4 published copies |
| XXS | 0.55214.02 | 1.77144.98 | 13.7120.40 | 4.02825.99 | 2.46315.89 | Checked against 4 published copies |
Checked against 3 published copies
Notes for 2-1/2" pipe
STD and XS, stainless, weight and what's not shown
- STD and Sch 40 are the same wall here (0.203"). They part above NPS 10.
- XS and Sch 80 are the same wall here (0.276"). They part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 2.875").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina), Metal Supermarkets.