Pipe schedule chart
4" pipe schedule
NPS 4 (DN 100) pipe is 4.500" outside diameter in every schedule. Schedule 40 has a 0.237" wall and a 4.026" ID; Schedule 80 has a 0.337" wall and a 3.826" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
4.500"114.30 mm
NPS 4 · DN 100
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.0832.11 | 4.334110.08 | 3.925.83 | 1.1527.43 | 14.75395.18 | Checked against 4 published copies |
| Sch 10 · 10S | 0.1203.05 | 4.260108.20 | 5.628.36 | 1.65110.65 | 14.25391.96 | Checked against 3 published copies |
| STD · Sch 40 · 40S | 0.2376.02 | 4.026102.26 | 10.8016.07 | 3.17420.48 | 12.73082.13 | Checked against 4 published copies |
| XS · Sch 80 · 80S | 0.3378.56 | 3.82697.18 | 15.0022.32 | 4.40728.44 | 11.49774.17 | Checked against 4 published copies |
| Sch 120 | 0.43811.13 | 3.62492.05 | 19.0228.30 | 5.58936.06 | 10.31566.55 | Checked against 4 published copies |
| Sch 160 | 0.53113.49 | 3.43887.33 | 22.5333.53 | 6.62142.72 | 9.28359.89 | Checked against 3 published copies |
| XXS | 0.67417.12 | 3.15280.06 | 27.5741.02 | 8.10152.27 | 7.80350.34 | Checked against 4 published copies |
Checked against 3 published copies
- Sch 160: Project Materials prints 0.674"; the other copies print 0.531".
Notes for 4" pipe
STD and XS, stainless, weight and what's not shown
- STD and Sch 40 are the same wall here (0.237"). They part above NPS 10.
- XS and Sch 80 are the same wall here (0.337"). They part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 4.500").
- Not shown: Sch 60 (only Engineers Edge prints it, 0.281"); Sch 140 (only Project Materials prints it, 0.531").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina), Metal Supermarkets.