Pipe schedule chart
5" pipe schedule
NPS 5 (DN 125) pipe is 5.563" outside diameter in every schedule. Schedule 40 has a 0.258" wall and a 5.047" ID; Schedule 80 has a 0.375" wall and a 4.813" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
5.563"141.30 mm
NPS 5 · DN 125
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.1092.77 | 5.345135.76 | 6.369.46 | 1.86812.05 | 22.438144.76 | Checked against 4 published copies |
| Sch 10 · 10S | 0.1343.40 | 5.295134.49 | 7.7811.57 | 2.28514.74 | 22.020142.07 | Checked against 3 published copies |
| STD · Sch 40 · 40S | 0.2586.55 | 5.047128.19 | 14.6321.77 | 4.30027.74 | 20.006129.07 | Checked against 4 published copies |
| XS · Sch 80 · 80S | 0.3759.53 | 4.813122.25 | 20.8030.95 | 6.11239.43 | 18.194117.38 | Checked against 4 published copies |
| Sch 120 | 0.50012.70 | 4.563115.90 | 27.0640.27 | 7.95351.31 | 16.353105.50 | Checked against 4 published copies |
| Sch 160 | 0.62515.88 | 4.313109.55 | 32.9949.10 | 9.69662.55 | 14.61094.26 | Checked against 3 published copies |
| XXS | 0.75019.05 | 4.063103.20 | 38.5957.43 | 11.34073.16 | 12.96583.65 | Checked against 4 published copies |
Checked against 3 published copies
- Sch 160: Project Materials prints 0.750"; the other copies print 0.625".
Notes for 5" pipe
STD and XS, stainless, weight and what's not shown
- STD and Sch 40 are the same wall here (0.258"). They part above NPS 10.
- XS and Sch 80 are the same wall here (0.375"). They part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 5.563").
- Not shown: Sch 140 (only Project Materials prints it, 0.625").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina), Metal Supermarkets.