Edge deforms or overheats
Sandvik, Mitsubishi and Iscar all say: lower the speed and feed; use a harder, more heat-resistant grade; get more coolant to the edge.
What you see
The edge sags, bulges or glows: the corner looks pushed down or out. Size and finish go off fast.
Causes and what to change
Every fix here is from Sandvik, Mitsubishi and Iscar's troubleshooting guides, unless marked. Change one thing at a time.
Too much heat and pressure: speed and feed too high
Lower the speed and feed
If the edge is pushed down, lower the feed first; if it bulges at the flank, the speed.
Use a more open, positive geometry
Only Sandvik and Mitsubishi
Take a lighter cut
Only Mitsubishi and Iscar
A grade too soft for the heat
Use a harder, more heat-resistant grade
Too little coolant
Get more coolant to the edge
Iscar: raise the coolant pressure.
Other changes the makers name
Use a larger nose radius
Only Mitsubishi
Plastic deformation: who gives which fix
Plastic deformation: which maker gives which fix
| Fix | Sandvik | Mitsubishi | Iscar |
|---|---|---|---|
| Lower the speed and feed | ✓ | ✓ | ✓ |
| Use a harder, more heat-resistant grade | ✓ | ✓ | ✓ |
| Get more coolant to the edge | ✓ | ✓ | ✓ |
| Use a more open, positive geometry | ✓ | ✓ | – |
| Take a lighter cut | – | ✓ | ✓ |
| Use a larger nose radius | – | ✓ | – |
Work it out
Often comes with
Sources
Sources4
- Sandvik Coromant — Troubleshooting in turning (archived Dec 4, 2024)
- Mitsubishi Materials — Trouble shooting for turning (archived Jul 10, 2026)
- Mitsubishi Materials — Causes of tool damage (types of cutting edge damage and solutions)
- ISCAR — ISO turn inserts wear troubleshooting
Written in our own words from each maker's troubleshooting guide.