Inserts wear out fast
Sandvik, Mitsubishi and Iscar all say: lower the cutting speed; use a harder, more wear-resistant grade.
What you see
Even wear land on the flank grows quickly; size drifts and finish fades well before the expected life.
Causes and what to change
Every fix here is from Sandvik, Mitsubishi and Iscar's troubleshooting guides, unless marked. Change one thing at a time.
Cutting speed too high
Lower the cutting speed
A grade too tough, without the wear resistance
Use a harder, more wear-resistant grade
Also named as causes
The guides name these, but give no change for them.
- Hard spots or inclusions in the material
Other changes the makers name
Get more coolant to the edge
Iscar: raise the pressure and check where it points.
Only Mitsubishi and Iscar
Use a sharper, more positive insert with a larger nose radius
Only Mitsubishi
Raise the feed if it is light
A feed too low rubs instead of cutting, and wears the flank.
Only Mitsubishi
Flank wear: who gives which fix
Flank wear: which maker gives which fix
| Fix | Sandvik | Mitsubishi | Iscar |
|---|---|---|---|
| Lower the cutting speed | ✓ | ✓ | ✓ |
| Use a harder, more wear-resistant grade | ✓ | ✓ | ✓ |
| Get more coolant to the edge | – | ✓ | ✓ |
| Use a sharper, more positive insert with a larger nose radius | – | ✓ | – |
| Raise the feed if it is light | – | ✓ | – |
Work it out
Often comes with
Sources
Sources4
- Sandvik Coromant — Troubleshooting in turning (archived Dec 4, 2024)
- Mitsubishi Materials — Trouble shooting for turning (archived Jul 10, 2026)
- Mitsubishi Materials — Causes of tool damage (types of cutting edge damage and solutions)
- ISCAR — ISO turn inserts wear troubleshooting
Written in our own words from each maker's troubleshooting guide.