Kennametal · chipbreaker for negative inserts

FS chipbreaker

Sharp finishing of high-temperature alloys.

One source: Kennametal, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO S.chipcutting edgebreaker grooveclearance 0°ISO groupS
The edge in section; its ISO groups. Not to scale.

What Kennametal prints

Insert
Negative
Made for
ISO S (superalloys and titanium)
Cutting area
finishing
Feed
0.08–0.25 mm/rev (.0031–.0098 in/rev)
Depth of cut
0.2–2.03 mm (.008–.08 in)
Edge
Precision ground, sharp

Kennametal prints its windows in inches; the millimetres are converted (×25.4, two places).

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

FS equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
MitsubishiFJISO S; finishingnot printedAlternative for finishing heat resistant and titanium alloys.

One source: Mitsubishi Materials, its own catalog

MitsubishiFSISO S; finishingnot printedFinishing difficult-to-cut materials (G class); the M-class FS is an alternative for finishing mild steel.

One source: Mitsubishi Materials, its own catalog

SecoMF1ISO S; finishing0.08–0.3 mm/revSemi-finishing and finishing of stainless, superalloys and titanium.

One source: Seco Tools, its own catalog

Why FS for heat-resistant superalloys (Inconel 718)

FS for heat-resistant superalloys (Inconel 718): Kennametal’s finishing geometry for ISO S.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Kennametal makes FS (negative) for S in finishing at 0.08–0.25 mm/rev (.0031–.0098 in/rev); edge: Precision ground, sharp. Sharp finishing of high-temperature alloys.

    One source: Kennametal, the maker of the chipbreaker , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), chip control geometries (pp. B30–B35) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists FS for ISO S, finishing. Kennametal’s own catalog is the authority for its geometry.

It agrees with Kennametal’s catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)