Mitsubishi · chipbreaker for negative inserts

FS chipbreaker

Finishing difficult-to-cut materials (G class); the M-class FS is an alternative for finishing mild steel.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO S.chipcutting edgebreaker grooveclearance 0°ISO groupS
The edge in section; its ISO groups. Not to scale.

What Mitsubishi prints

Insert
Negative
Made for
ISO S (superalloys and titanium)
Alternative for
ISO P (steel)
Cutting area
finishing
Edge
Large rake, precision (G class) sharp edge

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

FS equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalFSISO S; finishing0.08–0.25 mm/revSharp finishing of high-temperature alloys.

One source: Kennametal, its own catalog

KennametalLFISO S; finishing0.13–0.51 mm/revFinishing stainless and high-temperature alloys.

One source: Kennametal, its own catalog

SecoMF1ISO S; finishing0.08–0.3 mm/revSemi-finishing and finishing of stainless, superalloys and titanium.

One source: Seco Tools, its own catalog

Why FS for heat-resistant superalloys (Inconel 718)

FS for heat-resistant superalloys (Inconel 718): Mitsubishi’s finishing geometry for ISO S.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Mitsubishi makes FS (negative) for S (an alternative for P) in finishing; edge: Large rake, precision (G class) sharp edge. Finishing difficult-to-cut materials (G class); the M-class FS is an alternative for finishing mild steel.

    One source: Mitsubishi Materials, the maker of the chipbreaker , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists FS for ISO P, finishing. Mitsubishi Materials’ own catalog is the authority for its geometry.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)