Mitsubishi · chipbreaker for negative inserts
GJ chipbreaker
Alternative for rough cutting of difficult-to-cut materials.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Insert
- Negative
- Made for
- ISO S (superalloys and titanium)
- Cutting area
- roughing
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
GJ equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Seco | MR3 | ISO S; roughing | 0.2–0.6 mm/rev | Medium-rough and rough machining of superalloys, titanium, stainless and hardened steel. | One source: Seco Tools, its own catalog |
| Seco | MR4 | ISO S; roughing | 0.15–0.5 mm/rev | Difficult superalloy and titanium work: intermittent cuts and raw surfaces. | One source: Seco Tools, its own catalog |
Why GJ for heat-resistant superalloys (Inconel 718)
GJ for heat-resistant superalloys (Inconel 718): Mitsubishi’s roughing geometry for ISO S.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi makes GJ (negative) for S in roughing. Alternative for rough cutting of difficult-to-cut materials.
One source: Mitsubishi Materials, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: chip breaker classification (pp. A046–A070) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists GJ for ISO S, heavy roughing. Mitsubishi Materials’ own catalog is the authority for its geometry.
- The cross-reference lists it for heavy roughing; Mitsubishi Materials gives roughing.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)