Seco · chipbreaker for negative inserts
MR4 chipbreaker
Difficult superalloy and titanium work: intermittent cuts and raw surfaces.
One source: Seco Tools, its own catalog
What Seco prints
- Insert
- Negative
- Made for
- ISO S (superalloys and titanium)
- Cutting area
- medium, roughing
- Feed
- 0.15–0.5 mm/rev (.0059–.0197 in/rev)
- Depth of cut
- 1.5–7 mm (.059–.276 in)
- Edge
- Negative T-land, extremely high edge strength
Source: Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)
MR4 equivalents
Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.
| Maker | Chipbreaker | In common | Feed | What its maker says | Source |
|---|---|---|---|---|---|
| Kennametal | MS | ISO S; medium | 0.13–0.36 mm/rev | Medium machining, sharp edge, stainless and high-temperature alloys. | One source: Kennametal, its own catalog |
| Kennametal | P | ISO S; medium | 0.15–0.51 mm/rev | Medium machining of steel, stainless and high-temperature alloys. | One source: Kennametal, its own catalog |
| Kennametal | UP | ISO S; medium | 0.2–0.64 mm/rev | Medium machining of stainless and high-temperature alloys. | One source: Kennametal, its own catalog |
| Mitsubishi | GJ | ISO S; roughing | not printed | Alternative for rough cutting of difficult-to-cut materials. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | MS | ISO S; medium | not printed | First recommendation for medium cutting of difficult-to-cut materials; alternative for stainless. | One source: Mitsubishi Materials, its own catalog |
| Mitsubishi | RS | ISO S; roughing | not printed | First recommendation for rough cutting of difficult-to-cut materials; alternative for stainless; the positive land resists welding. | One source: Mitsubishi Materials, its own catalog |
Why MR4 for heat-resistant superalloys (Inconel 718)
MR4 for heat-resistant superalloys (Inconel 718): Seco’s medium and roughing geometry for ISO S.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Seco makes MR4 (negative) for S in medium, roughing at 0.15–0.5 mm/rev (.0059–.0197 in/rev); edge: Negative T-land, extremely high edge strength. Difficult superalloy and titanium work: intermittent cuts and raw surfaces.
One source: Seco Tools, the maker of the chipbreaker , sources [4]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)
What the cross-reference says
Mitsubishi’s chipbreaker comparison table, a compilation, lists MR4 for ISO K, S, heavy roughing. Seco Tools’ own catalog is the authority for its geometry.
- The cross-reference lists it for K; Seco Tools lists S.
- The cross-reference lists it for heavy roughing; Seco Tools gives medium, roughing.
Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)