Seco · chipbreaker for negative inserts

MR3 chipbreaker

Medium-rough and rough machining of superalloys, titanium, stainless and hardened steel.

One source: Seco Tools, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO M, S and H.chipcutting edgebreaker grooveclearance 0°ISO groupMSH
The edge in section; its ISO groups. Not to scale.

What Seco prints

Insert
Negative
Made for
ISO M (stainless steel), S (superalloys and titanium), H (hardened steel)
Cutting area
medium, roughing
Feed
0.2–0.6 mm/rev (.0079–.0236 in/rev)
Depth of cut
1.5–7 mm (.059–.276 in)
Edge
Positive rake, very high edge strength

Source: Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)

MR3 equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalMSISO M, S; medium0.13–0.36 mm/revMedium machining, sharp edge, stainless and high-temperature alloys.

One source: Kennametal, its own catalog

KennametalPISO M, S; medium0.15–0.51 mm/revMedium machining of steel, stainless and high-temperature alloys.

One source: Kennametal, its own catalog

KennametalRPISO M; roughingnot printedRoughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided).

One source: Kennametal, its own catalog

KennametalUPISO M, S; medium0.2–0.64 mm/revMedium machining of stainless and high-temperature alloys.

One source: Kennametal, its own catalog

MitsubishiESISO M; mediumnot printedRight- or left-hand alternative for medium cutting of stainless.

One source: Mitsubishi Materials, its own catalog

MitsubishiGJISO S; roughingnot printedAlternative for rough cutting of difficult-to-cut materials.

One source: Mitsubishi Materials, its own catalog

MitsubishiGMISO M; mediumnot printedAlternative to LM and MM for stainless; notch-wear resistant for light to medium cuts.

One source: Mitsubishi Materials, its own catalog

MitsubishiMMISO M; medium0.15–0.46 mm/revFirst recommendation for medium cutting of stainless.

One source: Mitsubishi Materials, its own catalog

MitsubishiMSISO S; mediumnot printedFirst recommendation for medium cutting of difficult-to-cut materials; alternative for stainless.

One source: Mitsubishi Materials, its own catalog

MitsubishiRMISO M; roughingnot printedFirst recommendation for rough cutting of stainless; resists fracture in interrupted cuts.

One source: Mitsubishi Materials, its own catalog

Show 3 more equivalents
More of other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
MitsubishiRSISO S; roughingnot printedFirst recommendation for rough cutting of difficult-to-cut materials; alternative for stainless; the positive land resists welding.

One source: Mitsubishi Materials, its own catalog

SandvikMMISO M; mediumnot printedFirst choice for medium machining of stainless (T-Max P).

One source: Sandvik Coromant, its own catalog

SandvikMRISO M; roughingnot printedFirst choice for roughing stainless (T-Max P).

One source: Sandvik Coromant, its own catalog

Why MR3 for austenitic stainless (304, 316)

MR3 for austenitic stainless (304, 316): Seco’s medium and roughing geometry for ISO M.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Seco makes MR3 (negative) for M, S, H in medium, roughing at 0.2–0.6 mm/rev (.0079–.0236 in/rev); edge: Positive rake, very high edge strength. Medium-rough and rough machining of superalloys, titanium, stainless and hardened steel.

    One source: Seco Tools, the maker of the chipbreaker , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Seco Tools — Turning catalogue 2026.2: carbide chipbreakers (pp. 111–114) (archived Nov 16, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists MR3 for ISO K, S, heavy roughing. Seco Tools’ own catalog is the authority for its geometry.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)