Sandvik · chipbreaker for negative inserts

MR chipbreaker

First choice for roughing stainless (T-Max P).

One source: Sandvik Coromant, its own catalog

The cutting edge of a negative insert in section: the breaker groove behind the edge with a chip curling out of it, and the flank at 0° clearance; made for ISO M.chipcutting edgebreaker grooveclearance 0°ISO groupM
The edge in section; its ISO groups. Not to scale.

What Sandvik prints

Insert
Negative
Made for
ISO M (stainless steel)
Cutting area
roughing

Source: Sandvik Coromant — Turning Handbook C-1020-18: geometry and grade, first choice for T-Max P and CoroTurn 107 (p. 2) (archived Nov 16, 2026)

MR equivalents

Other makers’ chipbreakers for negative inserts that their own catalogs make for at least one of the same main ISO groups and cutting areas. Equivalent means the same job, not the same shape: check the feed window for your cut.

Other makers’ chipbreakers for the same job
MakerChipbreakerIn commonFeedWhat its maker saysSource
KennametalRPISO M; roughingnot printedRoughing stainless (MG-RP, double-sided); heavy roughing of steel, stainless and cast iron (MM-RP, single-sided).

One source: Kennametal, its own catalog

MitsubishiRMISO M; roughingnot printedFirst recommendation for rough cutting of stainless; resists fracture in interrupted cuts.

One source: Mitsubishi Materials, its own catalog

SecoM5ISO M; roughing0.3–0.7 mm/revRoughing with double-sided inserts at high feed in steel, stainless and cast iron.

One source: Seco Tools, its own catalog

SecoMR3ISO M; roughing0.2–0.6 mm/revMedium-rough and rough machining of superalloys, titanium, stainless and hardened steel.

One source: Seco Tools, its own catalog

SecoRR6ISO M; roughing0.3–1 mm/revVery easy-cutting single-sided roughing of stainless and steel.

One source: Seco Tools, its own catalog

Why MR for austenitic stainless (304, 316)

MR for austenitic stainless (304, 316): Sandvik’s roughing geometry for ISO M.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Sandvik makes MR (negative) for M in roughing. First choice for roughing stainless (T-Max P).

    One source: Sandvik Coromant, the maker of the chipbreaker , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Turning Handbook C-1020-18: geometry and grade, first choice for T-Max P and CoroTurn 107 (p. 2) (archived Nov 16, 2026)

What the cross-reference says

Mitsubishi’s chipbreaker comparison table, a compilation, lists MR for ISO P, M, heavy roughing. Sandvik Coromant’s own catalog is the authority for its geometry.

Source: Mitsubishi Materials USA — Insert Chip Breaker Comparison Table (archived Jul 14, 2024)