Class 400 spiral wound gasket dimensions

A Class 400 NPS 4 spiral wound gasket winds from 4.75" to 5.88" on a 7.00" centering ring. The four diameters of a spiral wound gasket with inner and centering rings, NPS 1/2 to 24. Each is checked against three published copies of the standard (two for the inner ring); a tag marks any size where they differ.

The Class 400 NPS 4 spiral wound gasket, face on, to scale: centering ring Ø7.00", winding Ø4.75"–5.88".centering ring Ø7.00"winding Ø4.75"–5.88"
The Class 400 NPS 4 spiral wound gasket, face on. To scale.
Units

Class 400 spiral wound gasket chart

Class 400 spiral wound gaskets: inner ring ID, winding ID and OD, centering ring OD by pipe size
NPSInner ring ID (inmm)Winding ID (inmm)Winding OD (inmm)Centering ring OD (inmm)Inner ring
1/2B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
3/4B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
1B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
1-1/4B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
1-1/2B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
2B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
2-1/2B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
3B16.5 has no Class 400 flange below NPS 4: use the Class 600 gasket
44.04102.64.75120.75.88149.27.00177.8Not required
55.05128.35.81147.67.00177.88.38212.7Not required
66.10154.96.88174.68.25209.69.75247.7Not required
88.10205.78.88225.410.38263.512.00304.8Not required
1010.05255.310.81274.612.50317.514.13358.8Not required
1212.10307.312.88327.014.75374.716.50419.1Not required
1413.50342.914.25362.016.00406.419.00482.6Not required
1615.35389.916.25412.818.25463.621.13536.6Not required
1817.25438.218.50469.920.75527.123.38593.7Not required
2019.25489.020.50520.722.75577.925.50647.7Not required
2423.25590.624.75628.727.00685.830.25768.4Not required

Per ASME B16.20, checked against Lamons, Flexitallic and APG. Winding 0.175" (4.45 mm) thick; rings 0.117–0.131". breakingchips.com/gaskets/spiral-wound/class-400/

Thickness

Show
Winding
0.175" (4.45 mm), uncompressed
Inner and centering rings
0.117–0.131" (2.97–3.33 mm), nominally 1/8"

The rings stop the winding crushing: the joint is made up when the flanges close on them. Winding: Flexitallic and Wermac; ring range: Lamons and Wermac.

When the inner ring is required

Show
  • Class 900 NPS 24, Class 1500 NPS 12–24 and Class 2500 NPS 4–12.
  • Any PTFE-filled winding, at every size.
  • Flexitallic also fits one to every flexible graphite gasket unless the buyer says not to.

Elsewhere it is optional, though many makers fit one by default: it keeps the winding from buckling inward and smooths the flow past the joint. Lamons, Flexitallic and APG all print these rules.

Sources

Sources5