ISCAR · uncoated carbide
IC08 insert grade
IC08 is ISCAR’s uncoated carbide grade (Uncoated) for ISO N10–N20, as ISCAR’s catalog prints it. Steel, stainless and high-temperature alloys at low speed; non-ferrous.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- uncoated carbide
- Coating
- Uncoated
- Substrate
- Tough submicron grain
- ISO N
- N10–N20 · non-ferrous
- Secondary
- ISO P, M, S (ISCAR names them in its text only)
- Operations
- turning, milling
IC08 equivalents by material
ISO N (non-ferrous)
Read at N15, the centre of ISCAR’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | N10–N20 | One source: Kennametal, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | N10–N20 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why IC08 for aluminum
IC08 for aluminum: rated N10–N20 by ISCAR.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC08 (uncoated carbide) for N10–N20: Steel, stainless and high-temperature alloys at low speed; non-ferrous.
One source: ISCAR, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC08 at M20, M30, N10, N20, S10, S20. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)