Insert grades · ISCAR

ISCAR insert grade chart

31 ISCAR insert grades, each as ISCAR’s own catalog prints it: 6 CVD-coated carbide, 21 PVD-coated carbide, 1 cermet and 3 uncoated carbide. The table gives each grade’s coating and ISO range; each page lists the other makers’ grades for the same class.

One source: ISCAR, its own catalog

The six ISO groups, with how many of the maker’s listed grades cover each: P 22, M 28, K 11, N 6, S 20, H 11.PMKNSH22281162011
ISCAR’s listed grades by ISO group.

ISCAR insert grades by type

ISCAR insert grades: type, coating and ISO range
GradeTypeCoatingISO range
IC635CVD-coated carbideCVD, TiN + TiC + TiNP30–P50 and M20–M40
IC4050CVD-coated carbideCVD, TiCN + Al2O3 + TiNP20–P50, M20–M30 and K20–K40
IC6015CVD-coated carbideCVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)M05–M25
IC6025CVD-coated carbideCVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)M15–M35
IC8250CVD-coated carbideCVD, TiCN + Al2O3 + TiNP10–P35 and M05–M20
IC9350CVD-coated carbideCVD, TiCN + alpha Al2O3 + TiNP20–P45 and M15–M30
IC228PVD-coated carbidePVD, AlTiN + TiNP25–P50, M30–M40, K20–K50, N20–N40 and S25–S30
IC250PVD-coated carbidePVD, TiCN + TiNP15–P35 and M20–M40
IC300PVD-coated carbidePVD, TiCNP20–P40, M20–M35 and S15–S30
IC328PVD-coated carbidePVD, TiCNP25–P40, M30–M40 and S20–S30
IC354PVD-coated carbidePVD, TiCNP20–P40 and M10–M30
IC507PVD-coated carbidePVD, TiCN + TiNP10–P30, M05–M20, S05–S20 and H05–H15
IC520PVD-coated carbidePVD, TiCN + TiNM05–M15, N05–N15 and S05–S20
IC804PVD-coated carbidePVD, AlTiN (SUMOTEC treated)S05–S15
IC806PVD-coated carbidePVD, AlTiN (SUMOTEC treated)S15–S25
IC807PVD-coated carbidePVD, TiAlN + TiN (SUMOTEC treated)P10–P30, M05–M20, K10–K30, S05–S20 and H05–H15
IC808PVD-coated carbidePVD, TiAlN/AlTiN + TiN (SUMOTEC)P15–P30, M20–M30, K20–K30, S10–S25 and H20–H30
IC830PVD-coated carbidePVD, AlTiN + TiN (SUMOTEC)P20–P40, M25–M35 and S15–S30
IC882PVD-coated carbidePVD, AlTiN + TiAlSiN + TiSiNM25–M40 and S20–S30
IC900PVD-coated carbidePVD, AlTiNP15–P30, M20–M30, K20–K30, S10–S25 and H20–H30
IC903PVD-coated carbidePVD, AlTiNP10–P20, M15–M25, K10–K20, S10–S20 and H10–H20
IC907PVD-coated carbidePVD, TiAlNP10–P30, M05–M20, K15–K30, N05–N20, S05–S20 and H05–H15
IC908PVD-coated carbidePVD, TiAlNP15–P30, M20–M30, K20–K30, S10–S25 and H20–H30
IC928PVD-coated carbidePVD, TiAlNP20–P40, M25–M35 and S15–S30
IC1007PVD-coated carbidePVD, TiAlNP10–P30, M05–M20, K20–K40, S05–S20 and H05–H15
IC1008PVD-coated carbidePVD, AlTiN + TiNP15–P25, M15–M30, K15–K30, S10–S20 and H15–H25
IC1028PVD-coated carbidePVD, TiAlN + TiNP20–P50 and M20–M40
IC30NcermetUncoatedP10–P30, M10–M20 and H10–H25
IC07uncoated carbideUncoatedM10–M20, N05–N20 and S10–S30
IC08uncoated carbideUncoatedN10–N20
IC20uncoated carbideUncoatedM10–M25, K10–K20, N05–N25, S05–S20 and H05–H15
Sources31