Mitsubishi · uncoated carbide
HTi10 insert grade
HTi10 is Mitsubishi’s uncoated carbide grade (Uncoated) for ISO K10–K20 and N10–N20, as Mitsubishi’s catalog prints it. Non-ferrous metals and non-metals; also suitable for cast iron.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- uncoated carbide
- Coating
- Uncoated
- Substrate
- WC-Co, 92.0 HRA
- ISO K
- K10–K20 · cast iron
- ISO N
- N10–N20 · non-ferrous
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Mitsubishi’s first choice
- Mitsubishi names HTi10 its first choice for aluminum alloys (e.g. 6061, 7075), stable conditions: finishing, medium and roughing.
- Mitsubishi names HTi10 its first choice for aluminum alloys (e.g. 6061, 7075), general conditions: finishing, medium and roughing.
- Mitsubishi names HTi10 its first choice for aluminum alloys (e.g. 6061, 7075), unstable conditions: finishing, medium and roughing.
One source: Mitsubishi Materials, its own catalog
Open the insert pickerHTi10 equivalents by material
Cast iron · K
Read at K15, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC20 | uncoated carbide | Uncoated | K10–K20 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | K05–K20 | One source: Kennametal, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why HTi10 for gray cast iron
HTi10 for gray cast iron: rated K10–K20 by Mitsubishi.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates HTi10 (uncoated carbide) for K10–K20: Non-ferrous metals and non-metals; also suitable for cast iron.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
Non-ferrous · N
Read at N15, the centre of Mitsubishi’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC08 | uncoated carbide | Uncoated | N10–N20 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | N10–N20 | One source: Kennametal, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why HTi10 for aluminum
HTi10 for aluminum: rated N10–N20 by Mitsubishi.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Mitsubishi rates HTi10 (uncoated carbide) for N10–N20: Non-ferrous metals and non-metals; also suitable for cast iron.
One source: Mitsubishi Materials, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists HTi10 at Z10. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)