Sandvik · uncoated carbide
H10 insert grade
H10 is Sandvik’s uncoated carbide grade (Uncoated) for ISO N01–N25, as Sandvik’s catalog prints it. Aluminum alloys, rough to finish turning.
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Type
- uncoated carbide
- Coating
- Uncoated
- ISO N
- N01–N25 (core N15) · non-ferrous
- Operations
- turning
Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
H10 equivalents by material
ISO N (non-ferrous)
Read at N15, the centre of Sandvik’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC08 | uncoated carbide | Uncoated | N10–N20 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | N10–N20 | One source: Kennametal, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | N10–N20 | One source: Mitsubishi Materials, its own catalog |
Why H10 for aluminum
H10 for aluminum: rated N01–N25 (core N15) by Sandvik.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Sandvik rates H10 (uncoated carbide) for N01–N25 (core N15): Aluminum alloys, rough to finish turning.
One source: Sandvik Coromant, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists H10 at K10, N01, S01. Sandvik Coromant’s own catalog is the authority for its grade.
- The cross-reference lists K10; Sandvik Coromant gives no K application (its range: N01–N25).
- The cross-reference lists S01; Sandvik Coromant gives no S application (its range: N01–N25).
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)