ISCAR · PVD-coated carbide
IC806 insert grade
IC806 is ISCAR’s PVD-coated carbide grade (PVD, AlTiN (SUMOTEC treated)) for ISO S15–S25, as ISCAR’s catalog prints it. High-temperature and titanium alloys at moderate to fairly high speed.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- PVD-coated carbide
- Coating
- PVD, AlTiN (SUMOTEC treated)
- Substrate
- Hard submicron
- ISO S
- S15–S25 · superalloys and titanium
- Operations
- turning, milling
IC806 equivalents by material
ISO S (superalloys and titanium)
Read at S20, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | S15–S25 (core S20) | One source: Sandvik Coromant, its own catalog |
| Seco | CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about S10–S20 | One source: Seco Tools, its own catalog |
Why IC806 for heat-resistant superalloys (Inconel 718)
IC806 for heat-resistant superalloys (Inconel 718): rated S15–S25 by ISCAR.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC806 (PVD-coated carbide) for S15–S25: High-temperature and titanium alloys at moderate to fairly high speed.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC806
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC806 at S10, S20. ISCAR’s own catalog is the authority for its grade.
- The cross-reference lists S10; ISCAR gives S15–S25.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)